Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.200 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.508 J/cm² Grade Count:15 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.200 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.620 J/cm² Grade Count:20 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.210 - 1.00 J/cm² @Temperature -30.0 - 30.0 °C |
0.999 - 4.76 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.582 J/cm² Grade Count:31 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Charpy Impact, Notched | 0.700 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
3.33 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.786 J/cm² Grade Count:7 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Charpy Impact, Notched | 0.600 - 1.00 J/cm² | 2.86 - 4.76 ft-lb/in² | Average value: 0.770 J/cm² Grade Count:15 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Charpy Impact, Notched | 0.300 - 1.00 J/cm² | 1.43 - 4.76 ft-lb/in² | Average value: 0.512 J/cm² Grade Count:8 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact, Notched | 0.300 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.480 J/cm² Grade Count:5 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact, Notched | 0.300 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
1.43 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.675 J/cm² Grade Count:4 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact, Notched | 0.300 - 1.00 J/cm² | 1.43 - 4.76 ft-lb/in² | Average value: 0.567 J/cm² Grade Count:3 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Charpy Impact, Notched | 1.00 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.00 J/cm² Grade Count:1 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |
|||
Charpy Impact, Notched | 0.400 - 1.00 J/cm² | 1.90 - 4.76 ft-lb/in² | Average value: 0.739 J/cm² Grade Count:21 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.500 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.717 J/cm² Grade Count:9 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact, Notched | 0.800 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
3.81 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.900 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Charpy Impact, Notched | 0.300 - 1.00 J/cm² | 1.43 - 4.76 ft-lb/in² | Average value: 0.638 J/cm² Grade Count:21 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Charpy Impact, Notched | 0.100 - 1.00 J/cm² @Temperature -40.0 - 30.0 °C |
0.476 - 4.76 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.476 J/cm² Grade Count:23 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 0.100 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.476 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.545 J/cm² Grade Count:32 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.100 - 1.00 J/cm² @Temperature -30.0 - 30.0 °C |
0.476 - 4.76 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 0.430 J/cm² Grade Count:22 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Charpy Impact, Notched | 0.270 - 1.00 J/cm² @Temperature -40.0 - -20.0 °C |
1.28 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.734 J/cm² Grade Count:10 |
Overview of materials for Nylon 6, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact, Notched | 0.200 - 1.00 J/cm² @Temperature -40.0 - 30.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 0.478 J/cm² Grade Count:50 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.500 - 1.00 J/cm² @Temperature -40.0 - -20.0 °C |
2.38 - 4.76 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:3 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Charpy Impact, Notched | 1.00 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.00 J/cm² Grade Count:1 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact, Notched | 1.00 - 1.00 J/cm² @Temperature -30.0 - -30.0 °C |
4.76 - 4.76 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.00 J/cm² Grade Count:1 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber This material is a lightweight plastic with low moisture absorption, and is impact resistant at low temperatures. Applications include electronic housings, valve pistons, and support rollers.Inform.. |
|||
Charpy Impact, Notched | 0.400 - 1.00 J/cm² | 1.90 - 4.76 ft-lb/in² | Average value: 0.767 J/cm² Grade Count:3 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.600 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
2.86 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 1.34 J/cm² Grade Count:15 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.350 - 1.00 J/cm² | 1.67 - 4.76 ft-lb/in² | Average value: 0.836 J/cm² Grade Count:7 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Charpy Impact, Notched | 0.200 - 1.00 J/cm² | 0.952 - 4.76 ft-lb/in² | Average value: 0.617 J/cm² Grade Count:6 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Charpy Impact, Notched | 0.290 - 1.00 J/cm² | 1.38 - 4.76 ft-lb/in² | Average value: 0.471 J/cm² Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Charpy Impact, Notched | 0.200 - 1.00 J/cm² @Temperature -30.0 - -20.0 °C |
0.952 - 4.76 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.480 J/cm² Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Charpy Impact, Notched | 0.170 - 1.00 J/cm² | 0.809 - 4.76 ft-lb/in² | Average value: 0.442 J/cm² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |