| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced |
| Manufacturer | BASF |
| Trade Name | Ultramid® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Bulk Density | 0.450 - 0.800 g/cc | 0.0163 - 0.0289 lb/in³ | |
| Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
| Water Absorption | 6.5 - 7.5 % | 6.5 - 7.5 % | Saturation; ISO 62 |
| Moisture Absorption at Equilibrium | 1.6 - 2.0 % | 1.6 - 2.0 % | 23°C; 50% RH; ISO 62 |
| Viscosity Measurement | 130 | 130 | ISO 307 |
| Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | restricted |
| Linear Mold Shrinkage, Flow | 0.0090 cm/cm | 0.0090 in/in | ISO 2577 |
| Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50 mm/min; ISO 527-1/-2 |
| Elongation at Break | <= 11.5 % | <= 11.5 % | Nominal, 50mm/min; ISO 527-1/-2 |
| Elongation at Yield | 8.0 % | 8.0 % | 50 mm/min; ISO 527-1/-2 |
| Modulus of Elasticity | 3.20 GPa | 464 ksi | ISO 527-1/-2 |
| Tensile Creep Modulus, 1000 hours | 2300 MPa @Strain <=0.500 % |
334000 psi @Strain <=0.500 % |
ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 295 °C | 563 °F | DIN 53765 |
| Maximum Service Temperature, Air | 110 °C | 230 °F | for 50% loss of tensile strength after 20000hr |
| 130 °C | 266 °F | for 50% loss of tensile strength after 5000hr | |
| 250 °C | 482 °F | ||
| Decomposition Temperature | >= 350 °C | >= 662 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm | IEC 60093 |
| Dielectric Constant | 4.0 @Frequency 1.00 Hz |
4.0 @Frequency 1.00 Hz |
IEC 60250 |
| Dissipation Factor | 0.040 @Frequency 1.00e+6 Hz |
0.040 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 600 V | 600 V | Test solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
| Zone 1 | 300 °C | 572 °F | Feed Zone |
| Zone 2 | 310 °C | 590 °F | Compression |
| Zone 3 | 315 °C | 599 °F | Metering-zone |
| Zone 4 | 315 °C | 599 °F | Nozzle |
| Melt Temperature | 315 °C | 599 °F | Optimal |
| 310 - 330 °C | 590 - 626 °F | Injection-molding/Extrusion | |
| Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | Injection-molding |
| 90.0 °C | 194 °F | Optimal | |
| Drying Temperature | 110 °C | 230 °F | |
| Dry Time | 8 hour | 8 hour | |
| Moisture Content | <= 0.030 % | <= 0.030 % | Optimal |
| <= 0.15 % | <= 0.15 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | BK 00464 | |
| Commercial Status | Europe | |
| Ignition Temperature | >470°C | ASTM D1929 |
| Peripheral screw speed | < 0.3 m/s |