| Category | Polymer , Thermoplastic , Nylon , Nylon 66 |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.14 g/cc | 0.0412 lb/in³ | DAM; ISO 1183 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 55.0 MPa @Temperature 23.0 °C |
7980 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 85.0 MPa @Temperature 23.0 °C |
12300 psi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Elongation at Break | 20 % @Temperature 23.0 °C |
20 % @Temperature 73.4 °F |
DAM; nominal; ISO 527 |
| 40 % @Temperature 23.0 °C |
40 % @Temperature 73.4 °F |
50mm/min; DAM; ISO 527 | |
| >= 50 % @Temperature 23.0 °C |
>= 50 % @Temperature 73.4 °F |
50%RH; nominal; ISO 527 | |
| Elongation at Yield | 4.0 % @Temperature 23.0 °C |
4.0 % @Temperature 73.4 °F |
DAM; ISO 527 |
| 25 % @Temperature 23.0 °C |
25 % @Temperature 73.4 °F |
50%RH; ISO 527 | |
| Tensile Modulus | 1.40 GPa @Temperature 23.0 °C |
203 ksi @Temperature 73.4 °F |
50%RH; ISO 527 |
| 3.10 GPa @Temperature 23.0 °C |
450 ksi @Temperature 73.4 °F |
DAM; ISO 527 | |
| Flexural Modulus | 2.80 GPa @Temperature 23.0 °C |
406 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
DAM; ISO 180/1A |
| 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 180/1A | |
| Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 262 °C | 504 °F | 10°C/min; DAM; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 70.0 °C | 158 °F | DAM; ISO 75-1/-2 |
| UL RTI, Electrical | 140 °C @Thickness 0.710 mm |
284 °F @Thickness 0.0280 in |
DAM; UL 746B |
| 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 140 °C @Thickness 3.00 mm |
284 °F @Thickness 0.118 in |
DAM; UL 746B | |
| UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.710 mm |
203 °F @Thickness 0.0280 in |
DAM; UL 746B |
| 110 °C @Thickness 3.00 mm |
230 °F @Thickness 0.118 in |
DAM; UL 746B | |
| 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
DAM; UL 746B |
| 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B | |
| 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
DAM; UL 746B | |
| Flammability, UL94 | V-2 @Thickness 0.710 mm |
V-2 @Thickness 0.0280 in |
DAM; IEC 60695-11-10 |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; IEC 60695-11-10 | |
| V-2 @Thickness 0.710 mm |
V-2 @Thickness 0.0280 in |
DAM; UL94 | |
| V-2 @Thickness 3.00 mm |
V-2 @Thickness 0.118 in |
DAM; UL94 | |
| V-2 @Thickness 1.50 mm |
V-2 @Thickness 0.0591 in |
DAM; UL94 | |
| Glow Wire Test | 725 °C @Thickness 1.50 mm |
1340 °F @Thickness 0.0591 in |
DAM; Ignition; IEC 60695-2-13 |
| 725 °C @Thickness 3.00 mm |
1340 °F @Thickness 0.118 in |
DAM; Ignition; IEC 60695-2-13 | |
| 725 °C @Thickness 0.710 mm |
1340 °F @Thickness 0.0280 in |
DAM; Ignition; IEC 60695-2-13 | |
| 850 °C @Thickness 0.710 mm |
1560 °F @Thickness 0.0280 in |
DAM; IEC 60695-2-12 | |
| 960 °C @Thickness 3.00 mm |
1760 °F @Thickness 0.118 in |
DAM; IEC 60695-2-12 | |
| 960 °C @Thickness 1.50 mm |
1760 °F @Thickness 0.0591 in |
DAM; IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Comparative Tracking Index | 600 V @Temperature 23.0 °C |
600 V @Temperature 73.4 °F |
DAM; UL 746A |
| >= 600 V @Temperature 23.0 °C |
>= 600 V @Temperature 73.4 °F |
DAM; UL 746A |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 290 °C | 554 °F | DAM; Optimum |
| 280 - 300 °C | 536 - 572 °F | DAM | |
| Mold Temperature | 70.0 °C | 158 °F | DAM; optimum |
| 50.0 - 90.0 °C | 122 - 194 °F | DAM | |
| Drying Temperature | 80.0 °C | 176 °F | DAM |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | DAM |
| Moisture Content | <= 0.20 % | <= 0.20 % | DAM |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Black Color | DAM |
| Forms | Pellets | DAM |
| Generic | Nylon 66 | DAM |
| Material Status | Current | DAM |
| Part Marking Code | >PA66< | ISO 11469; DAM |
| Polymer Family | Polyamide | DAM |
| Polymer Type | PA66 | DAM |
| Processing Method | Injection Molding | DAM |
| Product Category | Unreinforced Resins | DAM |
| Region Available - Global | Yes | DAM |
| Resin Identification | PA66 | ISO 1043; DAM |
| RoHS Compliance | Contact Manufacturer | DAM |