| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Glass Fiber Filled , Nylon 66, Heat Stabilized |
| Manufacturer | Eurotec |
| Trade Name | Tecomid® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
| Moisture Absorption | 1.30 % @Temperature 23.0 °C |
1.30 % @Temperature 73.4 °F |
50% RH; ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.0090 cm/cm | 0.0090 in/in | Eurotec |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 230 MPa | 33400 psi | ISO 527 |
| Elongation at Break | 2.5 % | 2.5 % | ISO 527 |
| Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527 |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
| 18.0 kJ/m² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | 90.0 kJ/m² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
| 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
| Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75 |
| Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
| Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
|
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
| Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
| Drying Temperature | 80.0 °C | 176 °F | |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
| Moisture Content | <= 0.20 % | <= 0.20 % | ISO 960 |
| Hold Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Low | |
| Injection Speed | Fast |