| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.41 g/cc | 0.0509 lb/in³ | ISO 1183 |
| Moisture Absorption |
0.200 %
<br>@Temperature 23.0 °C
|
0.200 % <br>@Temperature 73.4 °F
|
50% RH; ISO 960 |
| Linear Mold Shrinkage, Flow | 0.0040 cm/cm | 0.0040 in/in | Eurotec |
| Linear Mold Shrinkage, Transverse | 0.0040 cm/cm | 0.0040 in/in | Eurotec |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 130 MPa | 18900 psi | ISO 527 |
| Elongation at Break | 2.0 % | 2.0 % | ISO 527 |
| Tensile Modulus | 9.00 GPa | 1310 ksi | ISO 527 |
| Izod Impact, Notched (ISO) |
12.0
kJ/m² <br>@Temperature -30.0 °C
|
5.71
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
15.0
kJ/m² <br>@Temperature 23.0 °C
|
7.14
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 145 °C | 293 °F | ISO 75 |
| Deflection Temperature at 1.8 MPa (264 psi) | 140 °C | 284 °F | ISO 75 |
| Vicat Softening Point |
145
°C <br>@Load 5.10 kg
|
293
°F <br>@Load 11.2 lb
|
ISO 306 |
| Glow Wire Test |
850
°C <br>@Thickness 2.00 mm
|
1560
°F <br>@Thickness 0.0787 in
|
GWFI; IEC 60695 |
|
875
°C <br>@Thickness 2.00 mm
|
1610
°F <br>@Thickness 0.0787 in
|
GWIT; IEC 60695 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 270 - 310 °C | 518 °F | |
| Feed Temperature | 60.0 - 80.0 °C | 140 °F | Throat |
| Mold Temperature | 80.0 - 100 °C | 176 °F | |
| Drying Temperature | 120 °C | 248 °F | |
| Dry Time | 3.00 - 4.00 hour | 3.00 hour | |
| Moisture Content | <= 0.10 % | <= 0.10 % | ISO 960 |
| Hold Pressure | 60.0 - 120 MPa | 8700 psi |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | Low | ||
| Injection Speed | Medium - Fast |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+15 ohm | 1.00e+15 ohm | IEC 60093 |
| Comparative Tracking Index | 175 V | 175 V | Solution A; IEC 60112 |