Material Notes:
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid Prototyping and Rapid Manufacturing applications. Vero Family: Opaque rigid materials offering toughness, dimensional stability and great detail visualizationFields of Use: Consumer products, Toy, Telecommunications, Computers and Architecture fieldsInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.18 - 1.19 g/cc
0.0426 - 0.0430 lb/in³
Polymerized; ASTM D792
Water Absorption 1.5 - 2.2 %

@Time 86400 sec
1.5 - 2.2 %

@Time 24.0 hour
ASTM D570-98
Ash 0.21 - 0.22 %
0.21 - 0.22 %
USP281
Mechanical Properties Metric English Comments
Hardness, Rockwell M 73 - 76
73 - 76
Hardness, Shore D 83 - 86
83 - 86
Tensile Strength at Break 50.0 - 60.0 MPa
7250 - 8700 psi
ASTM D638-03
Elongation at Break 15 - 25 %
15 - 25 %
ASTM D638-05
Modulus of Elasticity 2.00 - 3.00 GPa
290 - 435 ksi
ASTM D638-04
Flexural Strength 60.0 - 70.0 MPa
8700 - 10200 psi
ASTM D790-03
Flexural Modulus 1.90 - 2.50 GPa
276 - 363 ksi
ASTM D790-04
Izod Impact, Notched 0.200 - 0.300 J/cm
0.375 - 0.562 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °C
113 - 122 °F
ASTM D648-07
Glass Transition Temp, Tg 48.0 - 50.0 °C
118 - 122 °F
DMA, E