| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.34 g/cc | 0.0484 lb/in³ | dry; ISO 1183 |
| Moisture Absorption | 1.50 % | 1.50 % | Sim. To ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | ISO 294-4 |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | ISO 294-4 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 115 MPa | 16700 psi | cond; ISO 527-1/-2 |
| 170 MPa | 24700 psi | dry; ISO 527-1/-2 | |
| Elongation at Break | 4.0 % | 4.0 % | dry; ISO 527-1/-2 |
| 5.8 % | 5.8 % | cond; ISO 527-1/-2 | |
| Tensile Modulus | 7.00 GPa | 1020 ksi | cond; ISO 527-1/-2 |
| 9.50 GPa | 1380 ksi | dry; ISO 527-1/-2 | |
| Flexural Strength | 185 MPa | 26800 psi | cond; ISO 178 |
| 260 MPa | 37700 psi | dry; ISO 178 | |
| Flexural Modulus | 6.30 GPa | 914 ksi | cond; ISO 178 |
| 8.50 GPa | 1230 ksi | dry; ISO 178 | |
| Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eU |
| 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU | |
| 8.00 J/cm² @Temperature 23.0 °C |
38.1 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU | |
| Charpy Impact, Notched | 0.900 J/cm² @Temperature -30.0 °C |
4.28 ft-lb/in² @Temperature -22.0 °F |
dry; ISO 179/1eA |
| 1.10 J/cm² @Temperature 23.0 °C |
5.23 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA | |
| 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | dry; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 66.0 µm/m-°C | 36.7 µin/in-°F | dry; ISO 11359-1/-2 |
| Melting Point | 250 °C | 482 °F | 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 243 °C | 469 °F | dry; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 215 °C | 419 °F | dry; ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | cond; IEC 60093 |
| >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | dry; IEC 60093 | |
| Surface Resistance | 1.50e+14 ohm | 1.50e+14 ohm | cond; IEC 60093 |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | cond; IEC 60243-1 |
| 40.0 kV/mm | 1020 kV/in | dry; IEC 60243-1 | |
| Comparative Tracking Index | 600 V | 600 V | cond; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Calculated Bio Based Carbon Content (%) | 70 | ASTM 6866 |