| Category | Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade , Polystyrene, Transparent Grade |
| Manufacturer | LG Chemical |
| Trade Name | GPPS |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.010 | 0.010 | Injection Molding |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
ASTM D955 |
| Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 (G) |
| 8.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
8.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 (I) | |
| 39 g/10 min @Load 10.0 kg, Temperature 220 °C |
39 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 (G) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength, Yield | 52.0 MPa @Thickness 3.20 mm |
7540 psi @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Elongation at Break | 4.0 % @Thickness 3.20 mm |
4.0 % @Thickness 0.126 in |
50mm/min; ASTM D638 |
| Tensile Modulus | 2.88 GPa @Thickness 3.20 mm |
418 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
| Flexural Yield Strength | 98.1 MPa @Thickness 3.20 mm |
14200 psi @Thickness 0.126 in |
15mm/min; ASTM D790 |
| Flexural Modulus | 3.27 GPa @Thickness 3.20 mm |
474 ksi @Thickness 0.126 in |
15mm/min; ASTM D790 |
| Izod Impact, Notched | 0.0981 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.184 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| 0.0981 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.184 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 95.0 °C @Thickness 6.40 mm |
203 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C @Thickness 6.40 mm |
190 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
| 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical with Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
| 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
||
| UL RTI, Mechanical without Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
| 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
||
| Flammability, UL94 | HB @Thickness >=1.50 mm |
HB @Thickness >=0.0591 in |
|
| HB @Thickness >=3.00 mm |
HB @Thickness >=0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | |
| Dielectric Strength | 42.0 kV/mm | 1070 kV/in | |
| Arc Resistance | 120 - 180 sec | 120 - 180 sec | ASTM D495 |
| Hot Wire Ignition, HWI | 7.0 - 15 sec @Thickness >=1.50 mm |
7.0 - 15 sec @Thickness >=0.0591 in |
|
| 15 - 30 sec @Thickness >=3.00 mm |
15 - 30 sec @Thickness >=0.118 in |
||
| High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness 1.50 mm |
60 - 120 arcs @Thickness 0.0591 in |
|
| >= 120 arcs @Thickness 3.00 mm |
>= 120 arcs @Thickness 0.118 in |
||
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 170 - 190 °C | 338 - 374 °F | Injection Molding |
| Middle Barrel Temperature | 180 - 200 °C | 356 - 392 °F | Injection Molding |
| Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
| Nozzle Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
| Melt Temperature | 190 - 220 °C | 374 - 428 °F | Injection Molding |
| Mold Temperature | 40.0 - 70.0 °C | 104 - 158 °F | Injection Molding |
| Drying Temperature | 80.0 °C | 176 °F | Injection Molding |
| Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | Injection Molding |
| Back Pressure | 29.4 - 58.8 MPa | 4260 - 8530 psi | Injection Molding |
| Screw Speed | 30 - 60 rpm | 30 - 60 rpm | Injection Molding |