| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.49 g/cc | 1.49 g/cc | ASTM D792 |
| Water Absorption | 1.0 % | 1.0 % | ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0070 in/in @Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 211 MPa @Thickness 3.20 mm |
30600 psi @Thickness 0.126 in |
5mm/min; ASTM D638 |
| Elongation at Break | 3.0 % @Thickness 3.20 mm |
3.0 % @Thickness 0.126 in |
5mm/min; ASTM D638 |
| Flexural Yield Strength | 294 MPa @Thickness 3.20 mm |
42700 psi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Flexural Modulus | 11.8 GPa @Thickness 3.20 mm |
1710 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
| Izod Impact, Notched | 1.37 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.57 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 31.0 µm/m-°C | 17.2 µin/in-°F | ASTM D696 |
| Melting Point | 220 °C | 428 °F | ASTM D3418 |
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C @Thickness 6.40 mm |
410 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
| UL RTI, Electrical | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
| UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
| UL RTI, Mechanical without Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
| Flammability, UL94 | HB @Thickness >=0.750 mm |
HB @Thickness >=0.0295 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Dielectric Strength | 22.0 kV/mm @Thickness 1.00 mm |
559 kV/in @Thickness 0.0394 in |
ASTM D149 |
| Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm |
15 - 30 sec @Thickness >=0.0295 in |
|
| High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.750 mm |
>= 120 arcs @Thickness 0.0295 in |
|
| High Voltage Arc-Tracking Rate, HVTR | 25.4 - 50.0 mm/min | 1.00 - 1.97 in/min |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Injection Molding |
| Middle Barrel Temperature | 260 - 285 °C | 500 - 545 °F | Injection Molding |
| Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
| Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
| Melt Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
| Mold Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection Molding |
| Dry Time | 4.00 - 5.00 hour | 4.00 - 5.00 hour | Injection Molding |