Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6 GF 33 PA6, 33% glass fibre.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
FeaturesPA 6 for injection moulding, chemically strengthened with 33% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby tools, gears, covers of electric appliances, cooling skrews of blowers, electromotors, carrying parts in the automotive industry. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
Viscosity Measurement 0.55 - 0.98
0.55 - 0.98
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Linear Mold Shrinkage, Transverse 0.0098 cm/cm
0.0098 in/in
Melt Flow 3.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
3.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 10.5 GPa
1520 ksi
Flexural Strength 230 MPa
33400 psi
Flexural Modulus 8.65 GPa
1250 ksi
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -20.0 °C
35.7 ft-lb/in²

@Temperature -4.00 °F
8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.40 J/cm²

@Temperature -20.0 °C
6.66 ft-lb/in²

@Temperature -4.00 °F
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
Vicat Softening Point 215 °C
419 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+11 ohm-cm
5.00e+11 ohm-cm
Surface Resistance 8.00e+13 ohm
8.00e+13 ohm
Dielectric Strength 20.0 kV/mm
508 kV/in
Comparative Tracking Index 575 V
575 V
Processing Properties Metric English Comments
Melt Temperature 250 - 280 °C
482 - 536 °F
Mold Temperature 70.0 - 90.0 °C
158 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi