| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
| Manufacturer | Polykemi AB |
| Trade Name | POLYfill |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | Across Flow; ISO 2577 |
| 0.012 - 0.014 cm/cm | 0.012 - 0.014 in/in | With Flow; ISO 2577 | |
| Melt Index of Compound | 15 g/10 min @Load 2.16 kg, Temperature 230 °C |
15 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | <= 24.0 MPa | <= 3480 psi | ISO/R527 |
| Elongation at Yield | 5.0 % | 5.0 % | ISO/R527 |
| Flexural Strength | <= 50.0 MPa | <= 7250 psi | ISO 178 |
| Flexural Modulus | 2.20 GPa @Temperature 23.0 °C |
319 ksi @Temperature 73.4 °F |
ISO 178 |
| Charpy Impact, Notched | 0.300 J/cm² @Temperature 23.0 °C |
1.43 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 80.0 °C | 176 °F | 120°C/h; ISO 75/1 |
| Vicat Softening Point | 97.0 °C @Load 5.001 kg |
207 °F @Load 11.03 lb |
50°C/h; ISO 306 |
| Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
| Glow Wire Test | 960 °C @Thickness 2.00 mm |
1760 °F @Thickness 0.0787 in |
IEC 695-2-1 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 180 - 220 °C | 356 - 428 °F | |
| Mold Temperature | 20.0 - 50.0 °C | 68.0 - 122 °F | |
| Drying Temperature | 70.0 - 80.0 °C | 158 - 176 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | in desiccant air dryer |
| 2 - 4 hour | 2 - 4 hour | in circulation dryer | |
| Injection Pressure | 40.0 - 110 MPa | 5800 - 16000 psi | |
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Holding Pressure () | 20-40 | % of injection pressure |
| Injection Speed () | Normal |