| Category | Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.37 g/cc | 0.0495 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 6.0 % @Thickness 2.00 mm |
6.0 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 1.90 % @Thickness 2.00 mm |
1.90 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity | 46970 cP @Shear Rate 5000 1/s, Temperature 305 °C |
46970 cP @Shear Rate 5000 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
| 58620 cP @Shear Rate 5000 1/s, Temperature 295 °C |
58620 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 74567 cP @Shear Rate 5000 1/s, Temperature 285 °C |
74567 cP @Shear Rate 5000 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| 119700 cP @Shear Rate 500 1/s, Temperature 305 °C |
119700 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 | |
| 154240 cP @Shear Rate 500 1/s, Temperature 295 °C |
154240 cP @Shear Rate 500 1/s, Temperature 563 °F |
ISO 11403-1 -2 | |
| 201130 cP @Shear Rate 500 1/s, Temperature 285 °C |
201130 cP @Shear Rate 500 1/s, Temperature 545 °F |
ISO 11403-1 -2 | |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 88 | 88 | 50%RH; ISO 2039-2 |
| 104 | 104 | DAM; ISO 2039-2 | |
| Hardness, Rockwell R | 117 | 117 | 50%RH; ISO 2039-2 |
| 124 | 124 | DAM; ISO 2039-2 | |
| Tensile Strength at Break | 130 MPa | 18900 psi | 50%RH; ISO 527-1/-2 |
| 200 MPa | 29000 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 3.4 % | 3.4 % | DAM; ISO 527-1/-2 |
| 5.0 % | 5.0 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 7.00 GPa | 1020 ksi | 50%RH; ISO 527-1/-2 |
| 10.0 GPa | 1450 ksi | DAM; ISO 527-1/-2 | |
| Shear Modulus | 0.6452 GPa @Temperature 150 °C |
93.58 ksi @Temperature 302 °F |
DAM; Dynamic; ISO 11403-1 -2 |
| 0.714 GPa @Temperature 110 °C |
104 ksi @Temperature 230 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.2377 GPa @Temperature 60.0 °C |
179.52 ksi @Temperature 140 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.8948 GPa @Temperature 10.0 °C |
274.82 ksi @Temperature 50.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 1.9612 GPa @Temperature -20.0 °C |
284.45 ksi @Temperature -4.00 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| 2.0275 GPa @Temperature -50.0 °C |
294.07 ksi @Temperature -58.0 °F |
DAM; Dynamic; ISO 11403-1 -2 | |
| Izod Impact, Notched (ISO) | 13.0 kJ/m² | 6.19 ft-lb/in² | DAM; ISO 180/1A |
| 17.0 kJ/m² | 8.09 ft-lb/in² | 50%RH; ISO 180/1A | |
| 10.0 kJ/m² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 180/1A | |
| 12.0 kJ/m² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 180/1A | |
| Charpy Impact Unnotched | 8.20 J/cm² | 39.0 ft-lb/in² | DAM; ISO 179/1eU |
| 9.30 J/cm² | 44.3 ft-lb/in² | 50%RH; ISO 179/1eU | |
| 7.00 J/cm² @Temperature -30.0 °C |
33.3 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| 7.30 J/cm² @Temperature -30.0 °C |
34.7 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | DAM; ISO 179/1eA |
| 1.60 J/cm² | 7.61 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 1.00 J/cm² @Temperature -30.0 °C |
4.76 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA | |
| Tensile Creep Modulus, 1 hour | 6800 MPa @Time 3600 sec |
986000 psi @Time 1.00 hour |
50%RH; ISO 899-1 |
| Tensile Creep Modulus, 1000 hours | 5100 MPa @Time 3.60e+6 sec |
740000 psi @Time 1000 hour |
50%RH; ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 107 µm/m-°C | 59.4 µin/in-°F | DAM; ISO 11359-1/-2 |
| Melting Point | 263 °C | 505 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 261 °C | 502 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 248 °C | 478 °F | DAM; ISO 75-1/-2 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
DAM; IEC 60695-11-10 | |
| Flame Spread | 13 mm/min @Thickness 1.00 mm |
0.51 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+11 ohm-cm | 1.00e+11 ohm-cm | 50%RH; IEC 60093 |
| >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | DAM; IEC 60093 | |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | 50%RH; IEC 60093 |
| 1.00e+15 ohm | 1.00e+15 ohm | DAM; ASTM D257 | |
| Dielectric Constant | 4.1 @Frequency 1.00e+6 Hz |
4.1 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 |
| 4.4 @Frequency 100 Hz |
4.4 @Frequency 100 Hz |
DAM; IEC 60250 | |
| 4.6 @Frequency 1.00e+6 Hz |
4.6 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
| 10.8 @Frequency 100 Hz |
10.8 @Frequency 100 Hz |
50%RH; IEC 60250 | |
| Dielectric Strength | 32.0 kV/mm | 813 kV/in | 50%RH; IEC 60243-1 |
| 38.0 kV/mm | 965 kV/in | DAM; IEC 60243-1 | |
| Dissipation Factor | 0.0070 @Frequency 100 Hz |
0.0070 @Frequency 100 Hz |
DAM; IEC 60250 |
| 0.015 @Frequency 1.00e+6 Hz |
0.015 @Frequency 1.00e+6 Hz |
DAM; IEC 60250 | |
| 0.065 @Frequency 1.00e+6 Hz |
0.065 @Frequency 1.00e+6 Hz |
50%RH; IEC 60250 | |
| 0.46 @Frequency 100 Hz |
0.46 @Frequency 100 Hz |
50%RH; IEC 60250 | |
| Comparative Tracking Index | 400 V | 400 V | DAM; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA66-GF30< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Europe | |
| Near East/Africa | ||
| Resin Identification | PA66-GF30 | |
| Special Characteristics | Heat stabilised or stable to heat | |
| UL recognition | UL | DAM |