| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® 73G15HSL BK363 Nylon 6
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.25 g/cc | 0.0452 lb/in³ | DAM; ISO 1183 |
| Water Absorption | 7.6 % @Thickness 2.00 mm |
7.6 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Moisture Absorption | 2.50 % @Thickness 2.00 mm |
2.50 % @Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Viscosity Test | 150 cm³/g | 150 cm³/g | DAM; ISO 307 1157 1628 |
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0080 cm/cm | 0.0080 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 80.0 MPa | 11600 psi | 50%RH; ISO 527-1/-2 |
| 130 MPa | 18900 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 2.3 % | 2.3 % | DAM; ISO 527-1/-2 |
| 10 % | 10 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 4.00 GPa | 580 ksi | 50%RH; ISO 527-1/-2 |
| 6.50 GPa | 943 ksi | DAM; ISO 527-1/-2 | |
| Charpy Impact Unnotched | 4.00 J/cm² | 19.0 ft-lb/in² | DAM; ISO 179/1eU |
| 7.00 J/cm² | 33.3 ft-lb/in² | 50%RH; ISO 179/1eU | |
| 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 0.600 J/cm² | 2.86 ft-lb/in² | DAM; ISO 179/1eA |
| 0.700 J/cm² | 3.33 ft-lb/in² | 50%RH; ISO 179/1eA | |
| 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA | |
| 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 110 µm/m-°C | 61.1 µin/in-°F | DAM; ISO 11359-1/-2 |
| Thermal Conductivity | 0.200 W/m-K | 1.39 BTU-in/hr-ft²-°F | of melt |
| Melting Point | 221 °C | 430 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 204 °C | 399 °F | DAM; ISO 75-1/-2 |
| Vicat Softening Point | 215 °C | 419 °F | DAM; 50°C/h 50N; ISO 306 |
| Flammability, UL94 | HB @Thickness 1.50 mm |
HB @Thickness 0.0591 in |
DAM; IEC 60695-11-10 |
| Flame Spread | 25 mm/min @Thickness 1.00 mm |
0.98 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
| Oxygen Index | 21 % | 21 % | DAM; ISO 4589-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 21.5 kV/mm | 546 kV/in | DAM; IEC 60243-1 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Additives | Lubricants | |
| Release agent | ||
| Delivery Form | Pellets | |
| Emission of organic compounds | 8.5 µgC/g | VDA 277; DS |
| Odour | class 4 | VDA 270; DS |
| Part Marking Code | >PA6-GF15< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA6-GF15 | |
| Special Characteristics | Heat stabilised or stable to heat |