| Category | Polymer , Thermoset , Epoxy |
| Manufacturer | Epoxy Technology |
| Trade Name | EPO-TEK® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Epoxy Technology EPO-TEK® 430 Epoxy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.02 g/cc | 1.02 g/cc | Part B |
| 3.56 g/cc | 3.56 g/cc | Part A | |
| Particle Size | <= 50 µm | <= 50 µm | |
| Viscosity | 300000 - 400000 cP | 300000 - 400000 cP | 1 rpm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 86 | 86 | |
| Tensile Modulus | 4.19 GPa | 608 ksi | Storage |
| Shear Strength | >= 11.7 MPa | >= 1700 psi | Die |
| >= 13.8 MPa | >= 2000 psi | Lap |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 28.0 µm/m-°C | 15.6 µin/in-°F | Below Tg |
| 144 µm/m-°C | 80.0 µin/in-°F | Above Tg | |
| Thermal Conductivity | 1.34 W/m-K | 9.30 BTU-in/hr-ft²-°F | |
| Maximum Service Temperature, Air | 250 °C | 482 °F | Continuous |
| 350 °C | 662 °F | Intermittent | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | Continuous |
| -55.0 °C | -67.0 °F | Intermittent | |
| Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min |
| Decomposition Temperature | 420 °C | 788 °F | Degradation Temperature |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 0.0050 ohm-cm | >= 0.0050 ohm-cm |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Ionic Impurities - Na (Sodium) | 5.0 ppm | 5.0 ppm | |
| Ionic Impurities - K (Potassium) | >= 1.0 ppm | >= 1.0 ppm | |
| Ionic Impurities - Cl (Chloride) | 33 ppm | 33 ppm |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min @Temperature 80.0 °C |
0.500 hour @Temperature 176 °F |
|
| 60.0 min @Temperature 60.0 °C |
1.00 hour @Temperature 140 °F |
||
| Pot Life | 180 min | 180 min | |
| Shelf Life | 12.0 Month @Temperature 25.0 °C |
12.0 Month @Temperature 77.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Amber | Part B |
| Brown Copper | Part A | |
| Consistency | Thick paste | |
| Ionic Impurities NH4 | 63 ppm | |
| Mix Ratio By Weight | 100:2.5 | |
| Number of Components | Two | |
| Weight Loss | 0.18% | 200°C |
| 0.45% | 300°C | |
| 0.57% | 250°C |