| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.22 g/cc | 1.22 g/cc | |
| Viscosity | 2000 - 4000 cP @Temperature 23.0 °C |
2000 - 4000 cP @Temperature 73.4 °F |
100 rpm |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 83 | 83 | |
| Tensile Modulus | 2.00 GPa | 290 ksi | Storage |
| Shear Strength | 5.23 MPa | 758 psi | Lap |
| >= 35.2 MPa | >= 5100 psi | Die |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 49.0 µm/m-°C | 27.2 µin/in-°F | Below Tg |
| 150 µm/m-°C | 83.3 µin/in-°F | Above Tg | |
| Maximum Service Temperature, Air | 200 °C | 392 °F | Continuous |
| 300 °C | 572 °F | Intermittent | |
| Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | Continuous |
| -55.0 °C | -67.0 °F | Intermittent | |
| Glass Transition Temp, Tg | >= 110 °C | >= 230 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
| Decomposition Temperature | 420 °C | 788 °F | Degradation Temperature |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.5464 @Wavelength 589 nm |
1.5464 @Wavelength 589 nm |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | |
| Dielectric Constant | 3.63 @Frequency 1000 Hz |
3.63 @Frequency 1000 Hz |
|
| Dissipation Factor | 0.0070 @Frequency 1000 Hz |
0.0070 @Frequency 1000 Hz |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Ionic Impurities - Na (Sodium) | 275 ppm | 275 ppm | |
| Ionic Impurities - K (Potassium) | 15 ppm | 15 ppm | |
| Ionic Impurities - Cl (Chloride) | 12 ppm | 12 ppm |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 30.0 min @Temperature 150 °C |
0.500 hour @Temperature 302 °F |
minimum |
| 60.0 min @Temperature 120 °C |
1.00 hour @Temperature 248 °F |
minimum | |
| Pot Life | 40320 min | 40320 min | |
| Shelf Life | 6.00 Month | 6.00 Month | refrigerated |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Clear/Light Yellow | before cure |
| Consistency | Pourable liquid | |
| Number of Components | Single | |
| Weight Loss | 0.38% | 200°C |
| 0.64% | 250°C | |
| 0.84% | 300°C |