Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.21 - 1.32 g/cc
0.0437 - 0.0477 lb/in³
Average value: 1.27 g/cc Grade Count:8
Filler Content 10.0 - 15.0 %
10.0 - 15.0 %
Average value: 12.0 % Grade Count:5
Water Absorption 0.100 - 0.250 %
0.100 - 0.250 %
Average value: 0.157 % Grade Count:3
Linear Mold Shrinkage 0.00300 - 0.00700 cm/cm
0.00300 - 0.00700 in/in
Average value: 0.00490 cm/cm Grade Count:8
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.6 - 72.4 MPa
8500 - 10500 psi
Average value: 64.5 MPa Grade Count:8
Elongation at Break 4.00 - 10.0 %
4.00 - 10.0 %
Average value: 7.44 % Grade Count:8
Modulus of Elasticity 2.41 - 3.65 GPa
350 - 530 ksi
Average value: 3.17 GPa Grade Count:8
Flexural Yield Strength 89.6 - 110 MPa
13000 - 16000 psi
Average value: 98.7 MPa Grade Count:8
Flexural Modulus 2.76 - 3.45 GPa
400 - 500 ksi
Average value: 3.00 GPa Grade Count:8
Izod Impact, Notched 0.534 - 0.801 J/cm
1.00 - 1.50 ft-lb/in
Average value: 0.601 J/cm Grade Count:8
Izod Impact, Unnotched 4.81 - 10.7 J/cm
9.00 - 20.0 ft-lb/in
Average value: 7.47 J/cm Grade Count:8
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 - 143 °C
280 - 290 °F
Average value: 141 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 132 - 138 °C
270 - 280 °F
Average value: 135 °C Grade Count:8
Flammability, UL94 HB
HB
Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 1.00e+16 ohm-cm
1.00e+14 - 1.00e+16 ohm-cm
Average value: 6.91e+15 ohm-cm Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 249 - 293 °C
480 - 560 °F
Average value: 271 °C Grade Count:3
Melt Temperature 288 - 316 °C
550 - 600 °F
Average value: 302 °C Grade Count:5
Mold Temperature 65.6 - 121 °C
150 - 250 °F
Average value: 93.3 °C Grade Count:8
Drying Temperature 121 °C
250 °F
Average value: 121 °C Grade Count:5
Moisture Content 0.0200 %
0.0200 %
Average value: 0.0200 % Grade Count:5
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:5
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:8