| Category | Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Hexion Bakelite™ 151733 Phenolic Formaldehyde Resin
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.45 g/cc | 0.0524 lb/in³ | ISO 1183 |
| Apparent Bulk Density | 0.640 g/cc | 0.0231 lb/in³ | ISO 60 |
| Linear Mold Shrinkage, Flow | 0.0076 cm/cm | 0.0076 in/in | Injection molding; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 50.0 MPa | 7250 psi | 5 mm/min; ISO 527 - 1/2 |
| Tensile Modulus | 7.50 GPa | 1090 ksi | 1 mm/min; ISO 527 - 1/2 |
| Flexural Strength | 90.0 MPa | 13100 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 8.00 GPa | 1160 ksi | ISO 178 |
| Compressive Strength | 225 MPa | 32600 psi | Test specimen flat tested; ISO 604 |
| Charpy Impact Unnotched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
| Charpy Impact, Notched | 0.160 J/cm² @Temperature 23.0 °C |
0.761 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 8.0 MPa | 120 °C | 248 °F | ISO 75-2 |
| Shrinkage | 0.560 % @Temperature 110 °C, Time 605000 sec |
0.560 % @Temperature 230 °F, Time 168 hour |
Injection molding; ISO 2577 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+11 ohm | 1.00e+11 ohm | IEC 60093 |
| Dielectric Constant | 10 @Frequency 100 Hz |
10 @Frequency 100 Hz |
IEC 60250 |
| Dielectric Strength | 22.0 kV/mm @Thickness 1.00 mm |
559 kV/in @Thickness 0.0394 in |
IEC 60243-P1 |
| Dissipation Factor | 0.38 @Frequency 100 Hz |
0.38 @Frequency 100 Hz |
IEC 60250 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Feed Temperature | 60.0 - 75.0 °C | 140 - 167 °F | Injection molding |
| Nozzle Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
| Melt Temperature | 80.0 - 100 °C | 176 - 212 °F | Injection molding |
| Mold Temperature | 160 - 190 °C | 320 - 374 °F | Injection molding |
| 160 - 190 °C | 320 - 374 °F | Compression molding | |
| Injection Pressure | >= 15.0 MPa | >= 2180 psi | Compression and injection cavity mold pressure |
| Back Pressure | 0.500 - 2.00 MPa | 72.5 - 290 psi | Injection molding |
| Cure Time | 0.167 - 0.333 min | 0.00278 - 0.00556 hour | Per 1 mm of wall thickness, injection molding |
| 0.333 - 0.667 min | 0.00556 - 0.0111 hour | Per 1 mm of wall thickness, compression molding |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chromatic Spectrum | Subdued Colors | |
| Creep Rupture Strength | Good | |
| Holding Pressure | Approximately 40-60% of injection pressure | |
| Media Resistance | Good | |
| Moisture Absorption | 64 mg | ISO 62, 24 hours at 23°C |
| Reserves by Peak Temperature | High | |
| Thermal Expansion | Slight |