Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Glass Fiber Filled
Manufacturer Lehmann & Voss & Co.
Trade Name LUVOCOM®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lehmann & Voss LUVOCOM® 1105-7251 PEEK, with glass fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, hydrolysis resistance, non flammable.Information provided by Lehmann & Voss & Co.KG
Physical Properties Metric English Comments
Specific Gravity 1.84 g/cc
1.84 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
23°C/24h
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 380 °C
15 g/10 min

@Load 11.0 lb,
Temperature 716 °F
Mechanical Properties Metric English Comments
Tensile Stress 90.0 MPa
13100 psi
Elongation at Yield 1.0 %
1.0 %
flexural
1.5 %
1.5 %
Modulus of Elasticity 14.5 GPa
2100 ksi
Flexural Strength 160 MPa
23200 psi
Flexural Modulus 13.0 GPa
1890 ksi
Charpy Impact Unnotched 2.10 J/cm²
9.99 ft-lb/in²
edgewise; ISO 179 1eU
Coefficient of Friction, Dynamic 0.32
0.32
Coefficient of Friction, Static 0.30
0.30
Thermal Properties Metric English Comments
CTE, linear 22.0 µm/m-°C
12.2 µin/in-°F
DIN 53752
Thermal Conductivity 0.500 W/m-K
3.47 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 250 °C
482 °F
260 °C
500 °F
short term
Vicat Softening Point 330 °C
626 °F
DIN ISO 306
Flammability, UL94 V-0
V-0
not recognized by UL
Electrical Properties Metric English Comments
Insulation Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
Processing Properties Metric English Comments
Processing Temperature 390 °C
734 °F
mass temp
Nozzle Temperature 360 - 380 °C
680 - 716 °F
Zone 1 360 - 370 °C
680 - 698 °F
Zone 2 380 - 390 °C
716 - 734 °F
Zone 3 390 - 400 °C
734 - 752 °F
Mold Temperature 170 - 200 °C
338 - 392 °F
Drying Temperature 120 °C

@Time 21600 - 28800 sec
248 °F

@Time 6.00 - 8.00 hour
or
150 °C

@Time 10800 - 21600 sec
302 °F

@Time 3.00 - 6.00 hour
Dehumidifying dryer
Descriptive Properties Value Comments
Color natural color