Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Permabond A1046 Anaerobic Retainer

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Permabond
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Permabond A1046 Anaerobic Retainer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and excellent durability, even under the most arduous conditions. Permabond A1046 helps joints resist vibration, fatigue and fretting corrosion, which allows machining tolerances to be relaxed and mechanical locking devices to be eliminated. Permabond A1046 will help reduce processing costs. Features & Benefits: Toughened Rapid cure Ideal when bonding dissimilar materials Improved fatigue life Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Viscosity 2500 cP

@Temperature 25.0 °C
2500 cP

@Temperature 77.0 °F
at 20 rpm vibration
9000 cP

@Temperature 25.0 °C
9000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Storage Temperature 5.00 - 25.0 °C
41.0 - 77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 35.0 MPa
5080 psi
steel collar and pin shear; ISO 10123
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Strength 11.0 kV/mm
279 kV/in
Processing Properties Metric English Comments
Cure Time 4.98 min

@Temperature 23.0 °C
0.0830 hour

@Temperature 73.4 °F
Brass, handling strength
7.02 min

@Temperature 23.0 °C
0.117 hour

@Temperature 73.4 °F
Zinc, handling strength
4.98 - 10.2 min

@Temperature 23.0 °C
0.0830 - 0.170 hour

@Temperature 73.4 °F
M10 steel, handling strength
15.0 min

@Temperature 23.0 °C
0.250 hour

@Temperature 73.4 °F
Brass, working strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
Stainless steel, handling strength
30.0 min

@Temperature 23.0 °C
0.500 hour

@Temperature 73.4 °F
M10 steel, working strength
60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Zinc, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
Stainless steel, working strength
1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
M10 steel, full strength
Descriptive Properties Value Comments
Appearance Green
Uncured
Maximum Gap Fill (mm) 0.25
Maximum Thread Size M30
Strength Retention 50% at 150°C
Relative to 0°C
80% at 100°C
Relative to 0°C
93% at 50°C
Relative to 0°C
Torque Strength (N m) 30
M10 steel, break
50
M10 steel, prevail
UV Fluorescence Yes
Uncured